Carbon Ferrochrome

Carbon Ferrochrome

Ferrochrome is divided into high carbon ferrochrome according to different carbon content, including loading grade ferrochrome (C≦10%), medium carbon ferrochrome (C≦4.0%), low carbon ferrochrome (C≦0.5%), micro-carbon ferrochrome (C≦0.15%), etc. Commonly used are chromium silicon alloy, chromium nitride and so on. Ferrochrome is mainly used as an alloy additive in steelmaking and used to be added in the late refining stage of steelmaking. Smelting stainless steel and other low carbon steel, must use low and micro carbon ferrochrome, so refined ferrochrome production has been relatively large-scale development. Due to the improvement of the steelmaking process, when AOD method (see refining outside the furnace) is used to produce stainless steel and other steel grades, carbon ferrochrome (mainly charging grade ferrochrome) is loaded into the furnace, so only low and micro-carbon ferrochrome is added in the later period to adjust the composition, so now the focus of ferrochrome production is refining carbon ferrochrome. The introduction of the "Steel industry Development Policy" is a major event in the development of China's steel industry, which will play an important guiding role in the future development of China's steel industry, and is an important cornerstone for promoting the healthy development of the steel industry.
Send Inquiry
Product Introduction
Products Description

Smelting by reducing electric furnace, using coke as reducing agent, silica or bauxite as flux. The slag composition is generally SiO227~33%, MgO30~34%, Al2O326~30%, Cr2O3< 9.0%. Due to the formation of chromium carbide, the product contains 4~9% carbon. The reduction furnace capacity of modern smelting ferrochrome is 10,000 ~ 48,000 KVA, which is generally closed and fixed, and the smelting power consumption is 3000~4000 kW · h/ton. The smelting furnace of silicon chromium alloy is similar to that of chromium iron reduction furnace, and the smelting method has two kinds of one-step method and two-step method. Smelting with chromite, silica, coke and flux in one step process. The two-step method uses carbon ferrochrome, silica and coke as raw materials for slag-free smelting, and the smelting process is roughly similar to that of ferrosilicon production. Smelting power consumption per ton 3000~4000 kW · h.

intro
1596438297790739

►Extraction method

1.Medium, low and micro-carbon ferrochrome is generally made of silicochrome alloy, chromite and lime as raw materials, refined and desilicated by 1500~6000 kVA electric furnace, and operated by high alkalinity slag (CaO/SiO2 is 1.6~1.8). Low - and micro-carbon ferrochrome is also produced by thermal blending on a large scale. In production, two electric furnaces are used, one smelting silicon chromium alloy, the other melting slag composed of chromium ore and lime. The refining reaction is carried out in two stages in two buckets :① After the slag of the slag furnace is injected into the first bucket, the silicon chromium alloy that has been preliminarily desiliconized in the other bucket is added. Due to the large excess amount of oxidizer in the slag and sufficient desiliconization, the micro-carbon ferrochrome with silicon content less than 0.8% and carbon content as low as 0.02% can be obtained. ② The molten slag (containing about 15% Cr2O3) after the reaction in the first ladle is moved to the second ladle, the silicochrome alloy (containing 45% silicon) made by the silicochrome electric furnace is heated into the slag, and the initial desiliconized silicochrome alloy (containing about 25% silicon) is obtained after the reaction, and further desiliconized is added into the first ladle, and the slag containing less than 2~3% Cr2O3 can be abandoned.

 

20150706090756

2.Oxygen blowing refining medium and low carbon ferrochrome, using liquid carbon ferrochrome as raw material, adding a small amount of lime and fluorite to the molten pool to make slag, adding silicon chromium alloy or ferrosilicon before iron extraction to recover the chromium in the slag. The blowing of micro-carbon ferrochrome is possible under a certain vacuum degree.

3.Vacuum solid state decarburization refining, using finely ground high-carbon ferrochrome as raw material, in which a part of the finely ground high-carbon ferrochrome is oxidized and calcined as an oxidizing agent, with water glass or other binder, pressed into a mass, after low temperature drying, heated and reduced in a car-bottom vacuum furnace at a vacuum degree of 0.5~10 mm Hg and a temperature of 1300~1400℃ for 35~50 hours. The microcarbon ferrochrome containing carbon less than 0.03% or even less than 0.01% can be obtained.

 

 

 

 


Product Picture

38b6ccfe36333f3ab20b1e77870985f

8491fa67068c325ab6c6c7cec3efe421

Our factory

 

5ed1ffd28f7fc396ca0901bf1594d11

workshop

6ce4e047c04ad9c137439ecb8194495

workshop

40dcff8450452e1d069a1f8bc8e4cff

workshop

b6837746f2c202f601b9988cb125685

workshop

 

 

Send Inquiry

whatsapp

Phone

E-mail

Inquiry